dc.description.abstractEnabling metallic-Li negative electrodes is motivated by a significant increase of energy density, both gravimetric and volumetric (Fig. 1), despite the excess of metallic Li accounted to ensure a stable potential. The projected gain in energy density for post-Li-ion batteries with metallic Li is twice than that possible to achieve with graphite, whereas with current and potential positive electrodes of Li-ion batteries it is about 30 % [1]. However, Li-metal as an anode is prone to dendritic growth and, therefore, is considered an unsafe option. It has been under investigation since early 1970s and the interest declined with the invention of Li-ion battery technology, which was considered safer alternative. However, recently interest in the metallic Li has been again on a sharp rise [2]. There is still insufficient fundamental understanding about the fundamental principles, governing electrochemical lithium plating/stripping, which often results in dendrite growth, electrolyte consumption, other undesired effects. [3] The present study aims to gain a comprehensive fundamental understanding of metallic-Li behaviour upon plating/stripping. As a first step, we performed post-mortem SEM analysis during the first two cycles in various electrolytes, in addition to studying the cycling performance in Li–Cu and symmetric Li–Li cells. Our post-mortem SEM study revealed that Li plates sporadically, where some of the regions are preferred for plating, despite ‘dead’ Li agglomeration on those particular spots, while the other regions are free of Li deposits (Fig. 2). The most interesting morphological changes are obtained during the initial stages of stripping and plating.en_US
dc.identifier.citationBillaud, J., McNulty, D., & Trabesinger, S. (2020). Morphological Peculiarities from Lithium Plating and Stripping [Abstract]. The 8th International Conference on Nanomaterials and Advanced Energy Storage Systems; Nazarbayev University; National Laboratory Astana; Institute of Batteries.en_US
dc.identifier.urihttp://nur.nu.edu.kz/handle/123456789/4985
dc.language.isoenen_US
dc.publisherThe 8th International Conference on Nanomaterials and Advanced Energy Storage Systems; Nazarbayev University; National Laboratory Astana; Institute of Batteriesen_US
dc.rightsAttribution-NonCommercial-ShareAlike 3.0 United States*
dc.rights.urihttp://creativecommons.org/licenses/by-nc-sa/3.0/us/*
dc.subjectnegative electrodesen_US
dc.subjectResearch Subject Categories::TECHNOLOGYen_US
dc.subjectpost-Li-ion batteriesen_US
dc.titleMorphological Peculiarities from Lithium Plating and Strippingen_US
dc.typeAbstracten_US
workflow.import.sourcescience

Files

Original bundle
Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
Abstract book INESS 2020_Part12.pdf
Size:
385.83 KB
Format:
Adobe Portable Document Format
Description:
Abstract
License bundle
Now showing 1 - 1 of 1
No Thumbnail Available
Name:
license.txt
Size:
6.28 KB
Format:
Item-specific license agreed upon to submission
Description:

Collections